  • Handbook of Workability and Process Design
    Astroloy ( UNS N13017 ) and alloy U-700 are the two most difficult to forge nickel-base alloys.
  • ZHWPD2003P139
    Astroloy ( UNS N13017 ) and alloy U-700 are the two most difficult to forge nickel-base alloys.
  • ZASMHBA0003993
    Faster strain rates lead to frictional heat buildup, nonuniform recrystallization, and metallurgical instabilities, and are also likely to cause radial-type ruptures, especially in high-c0 alloys such as Astroloy ( UNS N13017 ) and U-700.
  • ZNCTA2000P198
    Therefore, slow strain rates are typically used during the initial closed-die reductions of such alloys as Astroloy ( UNS N13017 ) and René 95 (Ni-14Cr-8Co3.5Mo-3.5W-3.5Nb-3.5Al-2.5Ti).
  • ZASMHBA0005411
    Figure 3 shows the predictions of dwell-time effects using this simple model on Astroloy ( UNS N13017 ) at 655 C (1211 F), which compare very well with the data.
  • ZASMHBA0003184
    Astroloy ( UNS N13017 ) and Alloy U-700 are the two most difficult to forge nickel-base alloys.
  • ZASMHBA0003835
    Table 25 UNS No. N13017 N07754 S67956 ...